A stage light aluminum substrate is a composite material formed by curing resin, aluminum foil, and copper foil together. The thermal expansion coefficients of the resin and of the aluminum and copper foils differ greatly, so under external force and heat the resulting stress distribution in the board is uneven. If water molecules and some low-molecular-weight substances are present in the pores of the flat-panel interface, considerable stress concentration will occur under thermal shock; if the adhesive bonds cannot withstand these internal damaging forces, bubbles will form at the weak interface between the copper foil and the substrate, or between substrate layers.
To improve the solder-dip resistance of stage light aluminum substrates, it is necessary to reduce factors that may damage the surface structure during sheet forming and high-temperature processing. Improvement methods mainly include surface treatment of copper foil and aluminum material, improvement of the resin adhesive, and control of pressure and temperature during pressing. Many articles have already discussed how to increase the bond strength between copper foil and adhesive; this article focuses mainly on the surface treatment of aluminum.
Stage Light Aluminum Substrate Processing
Increasing Product Added Value
At present, driven by the rapid development of industries such as LEDs, aluminum substrates have developed quickly. There are many opportunities here, and of course more challenges as well, such as how to meet higher heat dissipation requirements. It is believed that more and more domestic enterprises will catch up with advanced foreign technology, refine their own processes, and increase product added value through technological innovation and industrial cooperation.
Enhancing Peel Strength
The interfacial bond strength of aluminum is generally determined by two parts: first, the bond strength between aluminum and the treated aluminum base material (thermal-insulating adhesive or adhesive); second, the bonding force between the adhesive and the resin. If the adhesive can penetrate well into the surface layer of the aluminum body, and the treated aluminum surface can chemically cross-link with the main resin, a higher peel strength of the aluminum body can be ensured.
Surface treatment methods for aluminum include oxidation and drawing, both of which enhance adhesion by increasing the surface area. Generally speaking, oxidation provides a much larger specific surface area than drawing, but oxidation itself varies considerably. Those in the industry know that aluminum oxidation is controlled by many factors; if it is not well controlled, phenomena such as a loose oxide film may appear. At present, quality stability control during production is an urgent problem for many domestic aluminum-oxidation board enterprises.
The above is an introduction to the causes of delamination bubbles during processing of stage light aluminum substrates. If you would like to know more, please feel free to consult us.