Due to their own construction, aluminum substrates have the following characteristics: excellent thermal conductivity, copper bonding on one side, components can only be placed on the copper-bonded side, electrical wiring holes cannot be opened, and jumpers cannot be arranged on a single-sided board.
Usually, chip components, switching tubes and output rectifier tubes are placed on aluminum substrates, and heat is conducted away through the substrate, so the thermal resistance is very low and high reliability can be achieved. Transformers with a planar SMD (surface-mount) structure can also dissipate heat through the substrate, and their temperature rise is lower than that of conventional transformers. A transformer of the same specification using an aluminum substrate structure can obtain greater output power. Aluminum substrate jumpers can be handled by bridging. An aluminum substrate power supply generally consists of two printed boards, with the other board accommodating the control circuit, and the two boards are integrated together through a physical connection.
Because aluminum substrates have excellent thermal conductivity, small-batch manual soldering is rather difficult, as the solder cools too quickly and problems easily occur. There is a simple and practical method. Turn an ordinary clothes iron (one with temperature adjustment) upside down, fix it in place, set the temperature to about 150°C, place the aluminum substrate on the iron, heat it for a while, and then attach and solder the components according to the conventional method; the iron temperature should be one at which the components are easy to solder.