Products
Products
  • PCB aluminum substrate manufacturing
  • PCB aluminum substrate manufacturing
PCB aluminum substrate manufacturing
Mr. Gou: 15989872495
Ms. Huang: 13632953944
Email: mshpcb@vip.163.com

Product Details

PCB aluminum substrateThe manufacturing process for preventing board warping during the manufacturing process.

1. Engineering Design: Precautions for Printed Circuit Board Design:

a. The arrangement of laminates should be symmetrical, such as 6 layers. The thickness between layers 1-2 and 5-6 should be consistent with the number of layers in the laminates, otherwise the laminates are prone to warping.

b. Multilayer core boards and semi cured chips should be manufactured by the same supplier.

c. The areas of surface A and B on the circuit diagram should be as close as possible. If the A side is a large copper surface and the B side has only a few rows, the etched printed board is easily warped. If the area difference between the two sides is too large, some independent grids can be placed on the thin edge to balance it.

2. Drying board before cutting:

The purpose of drying (150 ℃, 8 ± 2 hours) the copper composite board before cutting is to remove the moisture inside the board and completely cure the resin inside the board, further eliminating residual stress inside the board and preventing board warping. At present, many double-sided and multi-layer boards still adhere to the step of forming the board before cutting or after drying. However, some board factories also have exceptions. At present, the drying time of PCB factories varies, ranging from 4-10 hours. It is recommended to decide based on the brand of the printed circuit board produced and the customer's requirements for warping. After drying, cutting into pieces or drying the whole fennel is feasible. It is recommended to cut it on a drying board. The inner panel should also be baked.

3. The warp and weft directions of the semi cured film:

After composite, the warpage shrinkage and strip shrinkage of the semi cured board are different. Otherwise, lamination can easily cause warping of the finished board, and even if the board is pressed dry, it is difficult to correct. The reasons for multi-layer warping are often caused by the inability to distinguish the warp and weft of laminated semi cured films and the stacking of layers.

How to distinguish latitude and longitude? The rolled semi cured plate is rolled along the longitudinal direction, with a width of strip. The long side of copper foil is latitudinal, and the short side is meridional. If you are unsure, please consult the manufacturer or supplier.

4. Stress relief after lamination:

After hot pressing and cold pressing, the multi-layer board is taken out, and the burrs are cut or ground off. Then, it is placed flat in an oven at 150 degrees Celsius for 4 hours to gradually release the internal stress of the board, and the resin is completely cured without omission.

5. During the electroplating process, the metal plate should be straightened:

For electroplating and graphic electroplating of ultra-thin multilayer boards ranging from 0.4mm to 0.6mm, specialized fixtures should be made. After clamping the fins on the automatic electroplating line, use a round rod to string the clips on the entire fin to straighten all the plates on the drum, so that the electroplated plates will not deform. If this measure is not taken, after electroplating a copper layer of 20 or 30 microns, the thin plate will bend and be difficult to repair.

6. Cooling of steel plate after hot air leveling:

PCB hot air cleaning is usually carried out after high-temperature impact in the soldering tank (about 250 degrees Celsius), and should be placed on marble or steel plate for natural cooling before being sent to the processor for cleaning. This is a very good anti warping board. Some factories, in order to improve the brightness of the surface of lead tin plates, immediately place the hot air plate into cold water after leveling it, and take it out for post-processing after a few seconds. This kind of thermal shock may cause warping, delamination, or bubbles in some models of plates. In addition, an air floating bed can be added to the equipment for cooling.

7. Warp knitting board processing:

In a well managed factory, 100% flatness will be checked during the final inspection. All non-conforming boards will be picked out and placed in an oven at a temperature of 150 degrees Celsius, under pressure for 3 to 6 hours, and then placed under natural cooling pressure. Then take out the board and perform a flatness check, which can save some boards. Some boards need to be baked two or three times to be evenly distributed. Shanghai Huabao agent pneumatic bending machine is used by Shanghai Bell to remedy circuit board warping with good results. If the above anti warping measures are not implemented, some boards will have no use for drying pressure and can only be scrapped.

That is all.PCB aluminum substrateIntroduction to methods to prevent warping during the manufacturing process. If you want to learn more information, please feel free to consult.

Online Inquiry

Recommended Products

We are a professional manufacturer specializing in high-thermal-conductivity & high-power single/double-sided aluminum-based PCBs, thermally separated copper-based PCBs, copper-aluminum composite boards and other metal core substrates.
Copyright © Shenzhen Mingsihai Electronic Technology Co., Ltd. | Aluminum PCB Manufacturer, Service Provider, Custom Prototype Pricing, FabricationGuangdong ICP No.19065800